T4003 Stainless Steel
GB Grade: 022Cr12Ni
Chemical Composition
| Grade |
Standard |
C |
Si |
Mn |
P |
S |
Cr |
Ni |
N |
Ti |
Nb |
| T4003 |
Industry Standard |
≤0.03 |
≤1.0 |
1.0-2.50 |
≤0.04 |
≤0.015 |
11~13 |
0.6-1.0 |
≤0.025 |
8*C-0.35 |
0.05-0.1 |
|
Target |
≤0.012 |
0.4 |
1.75 |
≤0.035 |
≤0.003 |
11.1 |
0.85 |
≤0.012 |
8*C-0.35 |
0.08 |
Mechanical Properties
| Grade |
Standard |
Yield Strength (MPa) |
Tensile Strength (MPa) |
Elongation (%) |
Hardness HBW |
| T4003 |
Industry Standard |
≥350 |
≥480 |
≥20 |
≤250 |
T4003 stainless steel is an economical grade with low chromium and low nickel content, offering good corrosion resistance. It fills the material gap between stainless steel and coated steel for applications requiring a certain level of corrosion resistance. With excellent weldability and formability, it is mainly used in railway freight car bodies, street sweepers, flue ducts, railings, and similar applications.